Impact Factor (2025): 6.9
DOI Prefix: 10.47001/IRJIET
The welding
process of AISI 1020 steel causes changes in microstructure and corrosion
resistance. The corrosion attack pattern occurring on the steel can be
evaluated by observing the corroded surface. This research aims to determine
the corrosion attack pattern on welded joints of AISI 1020 steel. Specimens of
AISI 1020 steel that have been welded and subjected to post-weld heat treatment
(PWHT). PWHT involves heating the specimens to temperatures of 400, 500, and
600°C with a holding time of 1 hour, followed by air cooling. The specimens,
both before and after PWHT, were tested for corrosion using polarization
techniques. The surface of the specimens after corrosion testing was observed
using a microscope. The observation results indicate the presence of pitting
corrosion on the specimen surfaces after the corrosion test.
Country : Indonesia
IRJIET, Volume 7, Issue 11, November 2023 pp. 585-588